Anyone able to debug this #3dPrinting issue?

The part has a large flat base and it is peeling up every five or so passes.

Do I have too much heat? Not enough?
PLA, 200 extruder, 60 bed

@M0YNG
Seems you figured this out already, but first layer height and a level bed is important for good adhesion. Also a clean bed, no fingerprints or greasy spots, though some beds and plastics are more sensitive than others.

First layer speed can also be a factor.

You usually want to keep the fan off on the first layer or first couple of layers.